Pitting Assessments

Training | Oct 7, 2024

Pitting corrosion poses a serious threat to the integrity of metallic structures, primarily due to its highly localised nature. Unlike uniform corrosion, which affects larger areas more predictably, pitting targets small, concentrated spots on a metal’s surface, leading to the formation of cavities or “pits” that can penetrate deeply into the material. Even when the overall mass loss is minimal, these concentrated pits can significantly weaken a structure, potentially resulting in sudden failures. One of the key challenges in managing pitting corrosion lies in accurately determining the size and depth of these pits. Due to their varied shapes and potential to extend below the surface, precise measurement is complex, making it essential for engineers to adopt a careful and thorough assessment approach. Assessments can be guided by standards such as API 579 / ASME FFS-1 Part 6, which addresses Fitness-for-Service evaluations of localised corrosion, and ASTM G46-94, which provides detailed guidance on examining and evaluating pitting corrosion.

 

Approach to Assessing Pitting Corrosion

 

A structured approach is crucial when assessing pitting corrosion, beginning with visual inspections. This involves examining the corroded surface under normal lighting conditions, sometimes using low-power magnification to identify areas where pits have developed. Capturing images of the affected areas can be beneficial for future comparisons, especially before and after removing corrosion products.

Following the initial inspection, it’s vital to clean the corroded surface to reveal the full extent of the pitting. This should be done carefully to avoid further damage to the underlying metal, using methods that remove corrosion deposits without excessively attacking the base material. During this cleaning process, physically probing the pits may help identify hidden or subsurface corrosion. However, if the equipment in question contains pressure, special care must be taken when probing. Reckless probing can risk perforation, which could lead to a sudden release of pressure and potential hazards. Once the surface is cleaned, a more detailed examination using low magnification can provide insight into the pits’ size, shape, and distribution.

 

Credit ASTM G46

Using Non-destructive Testing Techniques

 

In certain situations, non-destructive testing methods are particularly useful for identifying pits without damaging the material. Techniques such as radiographic testing can reveal internal defects through variations in X-ray absorption, though they may not be sensitive enough for smaller pits.

Ultrasonic testing is especially effective for detecting deeper pits and determining their size and location. This method works by transmitting sound pulses through a couplant into the metal, with the resulting echoes indicating flaws. Ultrasonics provide quick insights in field conditions, though reference standards are needed for accuracy. Other methods, such as penetrant testing, can detect surface-breaking defects by applying a dye that seeps into the pits and becomes visible under special lighting. However, these techniques generally provide less detail about pit depth and are more suited for initial detection rather than in-depth analysis.

Pitting on stainless steel piping

Measuring the Extent of Pitting

Determining the extent of pitting is essential for assessing how much the corrosion has compromised the material. Mass loss measurements can offer some insight into the overall severity of pitting, particularly when general corrosion is low. However, this method does not provide details about the depth of pits and is less suitable when the primary concern is localised damage.

Direct measurement techniques, such as using a depth gauge or similar device, can be employed to assess pit depths in a non-destructive manner. This involves positioning a calibrated probe at the lip of a pit and measuring the distance to its base. Care should be taken to ensure that the probe reaches the bottom of the pit accurately, avoiding false readings caused by the pit’s irregular shape or undercutting. This method is particularly suitable for field conditions, allowing engineers to assess corrosion impact without removing samples or causing further damage.

 

Credit ASTM G46 – 94

Reporting the Findings

Accurate and detailed reporting is essential when documenting pitting assessments. It is important to include information about the test conditions, such as the material’s metallurgical state, surface preparation, and environmental exposure. Reports should detail the characteristics of pits, including their size, shape, density, and depth, as well as any changes observed in the material’s mechanical properties. Statistical insights should also be included to provide a complete understanding of the impact of corrosion.

By following a methodical approach that combines visual, non-destructive testing, and statistical analysis, it is possible to understand pitting corrosion’s effects thoroughly. Utilising standards like API 579 / ASME FFS-1 Part 6 and ASTM G46-94 can guide engineers in making well-informed decisions about the suitability of materials for their intended environments and in taking proactive steps to prevent unexpected failures, ensuring the continued reliability and safety of critical structures.

 

 

Statistical and Mechanical Evaluations

Statistical analysis plays a crucial role in understanding pitting behaviour, especially when working with large data sets from multiple samples. Analysing the distribution of pit depths can help predict the likelihood of encountering more severe pitting over a larger area, assisting in risk assessments and informing inspection and maintenance schedules.

Changes in mechanical properties, such as tensile strength, fatigue resistance, or impact toughness, can also indicate the effects of pitting on material performance. When pitting density is high, these changes can provide a reliable measure of how the material’s integrity has been compromised. However, it is crucial to use carefully prepared samples to ensure accurate comparisons between corroded and non-corroded conditions.

Additional resources, such as Guide G16, provide detailed information on the subject for a more comprehensive understanding and in-depth techniques.

 

 

A more practical approach is to use API 579 /ASME FFS -1

 

API 579-1/ASME FFS-1 Part 6 focuses on the Assessment of Pitting, specifically addressing conditions like pitting corrosion that can significantly impact the integrity of pressure-containing equipment. This section is part of the broader API 579-1/ASME Fitness-for-Service (FFS) standard, which evaluates the structural integrity of equipment that has experienced degradation or damage.

Part 6 provides a detailed framework for assessing localised corrosion, such as pits or areas where material thickness has been reduced due to corrosive attack. The goal is to determine whether the equipment is fit for continued service despite these localised flaws and, if so, under what conditions. It helps engineers evaluate the impact of pitting on the pressure-retaining capability of components like pipelines, pressure vessels, and storage tanks.

 

When is Part 6 Used?

Part 6 is typically used when a pressure-retaining component has localised corrosion that could compromise its ability to contain pressure safely. It is particularly useful when pitting corrosion is identified during inspections, such as through visual, ultrasonic, or other non-destructive testing methods. The assessment is applied in situations where the depth, distribution, and severity of pits must be evaluated to determine the remaining strength of the equipment.

The procedure is often used in industries like oil and gas, chemical processing, and other sectors that rely on pressure vessels and piping. It allows for the continued operation of equipment with known flaws, provided that the remaining strength meets safety margins.

Key Principles of Part 6

  1. Assessment Methods: Part 6 outlines different levels of assessment, ranging from simpler screening methods to detailed analysis:
  2. Determining the Critical Pit Size: A key part of the assessment is determining the maximum acceptable depth and size of pits based on the material properties, design pressure, and other operational factors. This helps establish whether the equipment can safely withstand the internal pressure or if repairs are needed.
  3. Calculating Remaining Strength: Part 6 provides equations to calculate the remaining strength factor (RSF) of corroded components. This factor helps assess the residual strength of the component after accounting for the material loss due to corrosion. An RSF above a certain threshold indicates that the equipment can remain in service safely.
  4. Safety Margins: The standard integrates safety factors into the assessment, ensuring that even if the pits reduce the material thickness, there remains a buffer to account for uncertainties in corrosion rate, operational conditions, and material variability.
  5. Documentation and Inspection: Detailed documentation is required, including records of the inspection findings, calculations, and any assumptions used in the analysis. This ensures traceability and a clear understanding of how decisions about the equipment’s continued use were made.

 

 

API 579-1/ASME FFS-1 Part 6 is a structured approach for evaluating localised corrosion like pitting in pressure-retaining equipment. It is used when pitting is detected, to determine if the affected equipment can still operate safely or if repairs are needed. By assessing factors such as pit size, remaining strength, and safety margins, engineers can make informed decisions about the integrity and remaining life of their equipment, ensuring safe and efficient operation.

 

Find out more about our Fitness For Service Training here. 

 

Read the article on linkedin